Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Heat Shrink Film Water Vapor Permeability Coefficient Testing: Standards, Methods, and Applications

Water vapor permeability coefficient testing is essential for evaluating the moisture barrier performance of heat shrink films used in food, beverage, pharmaceutical, and industrial packaging. This article explains the principle of water vapor transmission rate (WVTR) measurement, the gravimetric and instrumental sensor methods defined by ASTM, ISO, GB, and JIS standards, specimen preparation requirements, and how the permeability coefficient is calculated and applied in quality control.

Technical Overview

Heat shrink films—typically produced from polyolefin (POF), polyethylene (PE), polyvinyl chloride (PVC), polyethylene terephthalate glycol (PET-G), or oriented polystyrene (OPS)—are uniaxially or biaxially oriented films that contract when exposed to heat, forming a tight, conforming package around a product. Because these films frequently serve as the primary or secondary moisture barrier for packaged goods, their ability to resist water vapor transmission directly affects shelf life, product appearance, corrosion protection, and label integrity.

Water vapor transmission rate (WVTR) quantifies the steady-state flow of water vapor through a unit area of film per unit time under controlled temperature and humidity, and is expressed in g/m²·24h. The water vapor permeability coefficient, expressed in g·cm/(cm²·s·Pa), is a thickness-normalized, material-intrinsic value derived from the WVTR, the mean specimen thickness, and the water vapor partial pressure difference across the specimen. Together, these two parameters allow packaging engineers to compare materials of different thicknesses, verify incoming film quality, and model moisture ingress into sealed packages.

Molecular orientation, crystallinity, thickness uniformity, and additive content—all of which are strongly influenced by the stretching and annealing steps used in shrink film manufacturing—affect permeation behavior. For this reason, WVTR testing of shrink films must follow standardized procedures, and measurements are commonly performed by accredited third-party laboratories using either gravimetric cup methods or high-sensitivity instrumental sensor methods.

Testing Samples

Specimens are taken from flat, unshrunk film rolls as representative samples of the material. Typical specimen forms accepted for testing include the following:

POF Shrink Films (Cross-Linked and Non-Cross-Linked)

Polyolefin shrink films, usually 12–25 µm thick and produced as three-layer or five-layer coextruded structures, dominate light-gauge retail and food multipack applications. Their moderate moisture barrier helps prevent frosting and dehydration of frozen or chilled products, making WVTR verification a routine incoming inspection item.

PVC Heat Shrink Films

PVC shrink films, typically 30–60 µm thick, offer high clarity and stiffness and are widely used for bottle overwraps, box wrapping, and printable shrink labels. PVC has a comparatively higher moisture permeability than polyolefin films, so the permeability coefficient is frequently specified in procurement documents.

PE Shrink Films (LDPE, LLDPE, and Heavy-Duty Grades)

Low-density and linear low-density polyethylene shrink films, ranging from approximately 50 µm to more than 200 µm, are used for beverage multipacks, pallet stabilization, and industrial bundling. Their greater thickness generally yields lower WVTR values, and heavy-duty grades for weather-exposed loads require particular attention to moisture barrier data.

PET-G and OPS Shrink Films and Sleeves

Multilayer Coextruded and High-Barrier Shrink Films

Structures incorporating ethylene-vinyl alcohol copolymer (EVOH) or polyamide (PA) barrier cores, including shrink bags and high-barrier casing films for meat and cheese, can achieve WVTR values below 1–2 g/m²·24h. High-sensitivity instrumental methods are generally required to measure such low transmission rates accurately.

Testing Items

The core deliverable of the test is a quantitative moisture barrier characterization of the shrink film, which typically includes the following items:

  • Water vapor transmission rate (WVTR) in g/m²·24h, measured at standard conditions such as 38°C/90% RH or 23°C/85% RH
  • Water vapor permeability coefficient in g·cm/(cm²·s·Pa), calculated from WVTR, mean thickness, and the partial pressure difference
  • Comparative WVTR assessment before and after the shrinkage (heat-treatment) process to quantify the effect of heat exposure on barrier properties
  • Thickness measurement and thickness uniformity verification as supporting data for the coefficient calculation
  • Comparative barrier evaluation of different film structures, suppliers, or production batches for supplier qualification purposes

Testing Methods

Two families of methods are internationally recognized: gravimetric (cup) methods, in which permeated water vapor is determined by mass change, and instrumental sensor methods, in which permeated vapor is quantified by an infrared, electrolytic, or humidity sensor. The selection depends on the expected transmission rate, required sensitivity, and applicable purchasing or regulatory specification.

Gravimetric Cup Method (Desiccant Method and Water Method)

The cup method per ASTM E96/E96M, ISO 2528, GB/T 1037, and JIS Z 0208 seals the specimen over a cup containing either anhydrous desiccant (dry-cup method) or distilled water (wet-cup method). The assembly is placed in a controlled temperature and humidity chamber, and the cup is weighed periodically. In the desiccant method, water vapor is absorbed from the humid chamber environment through the film into the cup and the mass gain is recorded; in the water method, water vapor escapes from the cup through the film into a drier environment and the mass loss is recorded. WVTR is obtained from the linear slope of mass change versus time once steady-state transmission is reached, typically after several days. The method is simple and inexpensive but has limited sensitivity for high-barrier films.

Modulated Infrared Sensor Method

The infrared sensor method per ASTM F1249, ISO 15106-2, and GB/T 26253 clamps the specimen between a humid chamber and a dry chamber. A dry carrier gas sweeps the permeated water vapor to a modulated infrared sensor whose signal is proportional to the water vapor concentration. The method offers high sensitivity, good repeatability, and shortened test cycles, and is the preferred technique for high-barrier multilayer shrink films with transmission rates below a few g/m²·24h. Instruments are calibrated using reference films of certified transmission rate.

Electrolytic Sensor Method

The electrolytic detection method per ISO 15106-3 and GB/T 21529 carries permeated water vapor into an electrolytic cell where it is absorbed and electrolyzed; the electrolysis current is directly proportional to the amount of water transported. This method also provides high sensitivity and stable long-term measurement, making it suitable for both medium- and high-barrier shrink film grades.

Humidity Sensor Method

The humidity sensor method per ISO 15106-1 monitors the time-dependent relative humidity rise in a dry chamber adjacent to the specimen and derives the transmission rate from the dynamic humidity response. It is a useful alternative when fast comparative screening of shrink film samples is required.

Specimen Conditioning and Coefficient Calculation

Prior to testing, specimens are conditioned at 23°C ± 2°C and 50% ± 5% RH in accordance with ISO 291, GB/T 2918, or ASTM D618, normally for at least 24 hours. Specimens must be flat, free of pinholes, creases, and wrinkles, and representative of the roll; at least three specimens per condition are recommended, with results reported as the mean and standard deviation. Film thickness is measured at multiple points per GB/T 6672 or ASTM D6988 to obtain the mean thickness used in the calculation. The permeability coefficient is calculated as the WVTR (converted to g/(cm²·s)) multiplied by the mean thickness in cm, divided by the water vapor partial pressure difference in Pa across the specimen. For example, at 38°C the saturated water vapor pressure is approximately 6.63 kPa, so a 90% RH versus dry-side gradient corresponds to about 5965 Pa; a film with a WVTR of 10 g/m²·24h and a thickness of 20 µm yields a permeability coefficient of approximately 3.9 × 10⁻¹⁵ g·cm/(cm²·s·Pa).

Applications

Water vapor transmission data for heat shrink films support design and quality decisions across a broad range of end uses:

  • Food packaging: shrink wrapping of frozen foods, pizza, bakery items, cheese blocks, and confectionery multipacks, where the film controls dehydration, moisture pickup, and frost formation
  • Beverage packaging: shrink bundling of cans and bottles and full-body shrink sleeves, where moisture resistance preserves label adhesion and print appearance
  • Pharmaceutical packaging: carton overwraps and outer shrink films for moisture-sensitive medicinal products, supporting shelf-life and stability objectives
  • Electronics packaging: shrink films for moisture-sensitive components and assemblies, where a verified low permeability coefficient contributes to corrosion prevention
  • Industrial packaging: heavy-duty shrink film for machinery, steel coils, and palletized goods exposed to humid transport and storage environments
  • Retail and print products: shrink wrapping of books, magazines, stationery, and promotional multipacks for surface protection and tamper evidence

FAQ

What is the difference between WVTR and the water vapor permeability coefficient?

WVTR is a specimen- and condition-dependent result describing how much vapor passes through one square meter of a specific film in 24 hours under defined temperature and humidity. The permeability coefficient removes the effects of thickness and pressure gradient, making it an intrinsic material property that allows fair comparison between films of different thicknesses tested under different conditions.

Which test condition is most commonly specified?

The tropical condition of 38°C with 90% RH is the most widely specified for shrink films, referenced by GB/T 1037 and common in ASTM E96/E96M and ASTM F1249 test protocols. Alternatives include 23°C/85% RH for temperate simulation, 37°C/90% RH for pharmaceutical contexts, and 40°C/90% RH for accelerated aging. The selected condition should always be stated in the test report.

Should the shrink film be tested before or after shrinking?

Material qualification is normally performed on flat, unshrunk film because orientation and crystallinity at this stage define the supplied material. However, because the heat-shrinking process can alter morphology and therefore permeability, it is good practice to also test specimens after simulated or actual shrinkage when the film is intended as the functional moisture barrier of the finished package.

Which method is best for high-barrier shrink films?

Instrumental sensor methods—modulated infrared (ASTM F1249, ISO 15106-2) and electrolytic (ISO 15106-3, GB/T 21529)—offer significantly higher sensitivity and shorter test times than gravimetric cups, and they are recommended for multilayer films with WVTR values in the range of tenths of a g/m²·24h. The gravimetric cup method remains a reliable reference approach for medium-barrier films and for laboratories without sensor instrumentation.

How does film thickness affect the reported results?

For a homogeneous film, WVTR is approximately inversely proportional to thickness, so doubling thickness roughly halves the transmission rate, while the calculated permeability coefficient remains constant. Deviations from this relationship in shrink films can indicate orientation gradients, crystallinity variation, or thickness non-uniformity, which is why thickness data should always accompany the test result.

How many specimens are required, and how are results reported?

A minimum of three specimens per test condition is recommended for both cup and instrumental methods. The test report should state the test standard, method, temperature and humidity, specimen thickness and test area, individual and mean WVTR values, the calculated permeability coefficient, and the saturated vapor pressure basis used in the calculation, ensuring full traceability and comparability of results.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time