Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Fishing Net Mesh Size Testing and Measurement

Fishing net mesh size testing determines the stretched mesh size, bar length, and dimensional deviation of knotted and knotless netting in accordance with ISO 3790 and related GB/T standards. Accurate mesh size measurement is essential for compliance with fisheries management regulations, fishing gear selectivity, and netting manufacturing quality control. This article explains the sample types, tested parameters, measurement procedures, calculation methods, and typical applications of professional fishing net mesh size testing.

Technical Overview

Mesh size is the fundamental dimensional parameter of a fishing net, directly governing catch selectivity, bycatch reduction, water flow through aquaculture enclosures, and compliance with minimum mesh size requirements imposed by fisheries management authorities. Because netting is an elastic, knitted or knotted textile structure, mesh dimensions change with moisture, tension, and relaxation history, so mesh size must be measured under strictly standardized conditions to yield comparable, defensible results.

Professional mesh size testing is primarily performed in accordance with ISO 3790, which specifies the determination of the length of mesh and the length of netting. Supporting references include ISO 139 for standard atmospheric conditioning of textile samples, together with GB/T and SC/T series national and industry standards for fishing gear materials, as well as buyer or contractual technical specifications.

  • Stretched mesh size: the internal distance, measured under defined tension, between the inner edges of two diagonally opposite knots or joints of a single mesh when it is extended in its longest direction.
  • Bar length (mesh leg): the length of one straight twine segment between two adjacent knots or joints; for knotted netting, the internal stretched mesh size corresponds to the sum of two opposing bar lengths.
  • Mesh deviation: the percentage difference between the measured average mesh size and the nominal mesh size specified in the product standard or purchase contract.

Testing may be carried out on knotted netting, knotless (raschel) netting, and finished fishing gear, and can be performed in both the dry state and the wet state, since many netting yarns, particularly polyamide, exhibit significant shrinkage or dimensional change after immersion in water.

Testing Samples

Knotted Netting Samples

Knotted netting includes single-knot and double-knot constructions produced from polyamide multifilament, polyamide monofilament, polyester, or polyethylene twisted twine. Samples are typically cut as panels of at least 500 mm by 500 mm, taken from representative positions of the production lot and kept well away from the selvage edges and any damaged or repaired meshes. The nominal mesh size, twine specification, knot type, and lot identification are recorded before conditioning.

Knotless (Raschel) Netting Samples

Knotless netting, manufactured by warp-knitting or raschel knitting from polyethylene, polypropylene, or polyamide yarn, has no discrete knots, so mesh size is expressed by the internal opening dimensions measured in both the N-direction (across the netting width) and the T-direction (along the netting length). Sample panels of comparable size are prepared with edges stabilized by temporary stitching or heat sealing to prevent unravelling before and during measurement.

Finished Net and Gear Samples

Complete or partially assembled fishing gear, such as trawl cod-ends, gillnets, trammel nets, purse seine panels, and aquaculture cage nets, may be tested directly. Measurement positions are selected from designated panels of the gear, avoiding hanging points, lashings, strengthening selvedges, and reinforced sections, so that the result represents the working mesh size of the netting itself.

Testing Items

Depending on the purpose of the evaluation, the following items are determined and reported:

  • Average stretched mesh size (internal measurement, dry and/or wet state)
  • Average bar length (mesh leg length) for knotted netting
  • Mesh size deviation from nominal value, expressed as a percentage
  • Mesh count, i.e., the number of meshes per unit length (meshes per meter or meshes per 100 meshes length)
  • Mesh uniformity, evaluated through the coefficient of variation among measurement series
  • Dimensional change after wetting, expressing shrinkage or elongation relative to the dry state

For regulatory compliance purposes, the reported average mesh size is compared against the minimum mesh size prescribed by the applicable fisheries management authority. For commercial acceptance, the measured value is compared against the tolerance band defined by the product standard or the purchase contract.

Testing Methods

Conditioning and Preparation

Prior to dry measurement, samples are relaxed free of tension, with kinks and creases gently removed by hand, and conditioned in the standard atmosphere specified in ISO 139, namely 20 ± 2 °C and 65 ± 4 % relative humidity, for a period sufficient to reach moisture equilibrium, typically not less than 24 hours. Samples must not be stretched, ironed, or otherwise distorted during preparation.

Dry-State Stretched Mesh Measurement

Following the principle of ISO 3790, a series of ten consecutive meshes is selected in the N-direction at a representative position of the panel. A standardized tension, appropriate to the twine linear density and sufficient to straighten the mesh bars and set the knots without elongating the twine, is applied so that the meshes open fully in a straight line. The total internal distance between the inner edge of the knot at the beginning of the first mesh and the inner edge of the knot at the end of the tenth mesh is measured with a steel rule or vernier caliper graduated to 1 mm or finer. The measurement is repeated for at least three series distributed across the length and width of the sample, and the stretched mesh size of each series is obtained by dividing the measured distance by ten.

Wet-State Measurement

To simulate service conditions, samples are fully immersed in clean fresh water at 20 ± 2 °C for a defined soaking period, drained without wringing, and measured using the same tensioning and reading procedure as for the dry state. Wet measurement is particularly significant for polyamide netting, which may shrink appreciably after immersion, and is often the reference condition for regulatory mesh size checks performed by enforcement authorities.

Wedge Gauge Verification

For rapid verification on knotless netting or in field conditions, a tapered flat wedge gauge may be inserted into the mesh under a defined load until it is firmly seated, and the mesh size is read directly at the contact line. This method provides a convenient screening value, while full laboratory measurement in accordance with ISO 3790 remains the reference procedure for certification and dispute resolution.

Calculation and Evaluation of Results

  • Average stretched mesh size = sum of all series mesh sizes divided by the number of series.
  • Deviation (%) = (average measured mesh size − nominal mesh size) / nominal mesh size × 100.
  • Coefficient of variation (%) = standard deviation of series results / average × 100, used to assess mesh uniformity.

Unless otherwise specified by the governing product standard or contract, commercial netting is commonly accepted when the average mesh size deviation falls within approximately ±2 % to ±5 % and mesh uniformity is satisfactory. For regulatory purposes, the measured average mesh size must not be smaller than the prescribed minimum mesh size for the fishing area and gear type concerned.

Applications

MESH size testing services are applied across the fisheries supply chain and regulatory framework, including:

  • Fisheries management compliance, verifying that commercial fishing gear meets minimum mesh size requirements designed to reduce the capture of juvenile fish and minimize bycatch.
  • Netting manufacturer quality control, validating knotting machine setup, heat-setting and stretching processes, and batch-to-batch consistency during production.
  • Incoming inspection by net and gear manufacturers, confirming that purchased netting matches the ordered nominal mesh size before fabrication into finished gear.
  • Trade acceptance and export inspection, providing objective dimensional data for netting transactions and customs clearance, often issued as test reports by accredited third-party laboratories.
  • Aquaculture engineering, selecting cage and enclosure netting with appropriate mesh dimensions for species containment, predator exclusion, and optimal water exchange.
  • Gear selectivity research and development, supplying accurate mesh size data for scientific experiments on catch composition and escape behavior.
  • Dispute resolution and arbitration, delivering traceable measurement results when mesh size claims arise between buyers, sellers, or regulatory bodies.

FAQ

What is the difference between bar length and stretched mesh size?

The bar length is the length of a single twine segment between two adjacent knots or joints, while the stretched mesh size is the internal distance between two diagonally opposite knots when the mesh is pulled open under defined tension. For knotted netting, the internal stretched mesh size corresponds to the combined length of two opposing bars, measured between the inner edges of the knots.

Should mesh size be measured dry or wet?

Both conditions can be measured and the state must always be stated in the report. Dry measurement after standard conditioning reflects the as-manufactured dimension, whereas wet measurement reflects the in-service dimension and is often the reference condition for regulatory enforcement, particularly for polyamide netting that shrinks in water.

How many meshes are measured and where?

The standard approach measures series of ten consecutive meshes at several positions distributed across the sample, avoiding selvages, damaged meshes, and reinforced areas. A minimum of three series is typical, and the reported mesh size is the average of all series results.

What tension is applied during measurement?

A standardized tension appropriate to the twine linear density is applied so that the mesh bars are straight and the knots are set, but the twine itself is not elongated. The same tension must be used for every series within a test to ensure comparability of results.

What tolerance is acceptable for mesh size?

Acceptance tolerances are defined by the applicable product standard or the purchase contract, and commonly fall within approximately ±2 % to ±5 % of the nominal mesh size. Where a regulatory minimum mesh size applies, the measured average must not fall below that minimum regardless of commercial tolerance.

How should samples be submitted for testing?

Samples should be submitted as flat netting panels of at least 500 mm by 500 mm, or as agreed representative sections of finished gear, clearly labeled with the nominal mesh size, twine or yarn specification, material, knot or knitting type, and lot number, together with the required measurement state, dry, wet, or both.

Why Choose ZKGX?

  • State-of-the-art analytical equipment